The production of single superphosphate (SSP) involves following operations:
(A) . The powdered rock phosphate (containing 30%-38% total POs) is mixed with sulphuric
acid (65%-75% H»SOa) to form a slurry.
(B) . The wet material is subjected to final curing, when some of the slow reactions reach a state of near completion and
the excess water evaporates. The curing time is 2-6 weeks
(C) . Solidification of the slurry in a den (denning), where continued reactions and crystallization of monocalcium
phosphate take place (time required 0.5 to 4 hours)
(D) . If granular SSP is desired, it can be granulated either before or after it is cured
Choose the correct answer from the options given below: